Editorial responsibility for this article rests with Wuhan Ooi Photoelectric Technology Co., Ltd. Written and reviewed by the Ooitech editorial team. See our editorial policy for how we write, where AI tools are used, and how to request a correction.

0BB Cell Technology: What Removing the Busbar Changes

Quick answer: A busbar carries current, and it does two other jobs as well: it gives the ribbon a wide solderable pad and it acts as the placement reference that locates the ribbon. Removing it is therefore a process decision rather than a printing decision. 0BB keeps the fingers and replaces the busbar with many thin wires, fixed in place by an embedded foil, a film, a dispensed adhesive, or a local weld plus adhesive. The four routes differ mainly in what holds the wire before lamination, and that difference decides whether a bad joint can be found before the module is built.

Look at the front of a conventional solar cell and the layout reads like a road network: thin parallel lines running the full width, crossed by a few much wider lines, with small metal patches where the wide lines meet the ribbon. The thin lines are fingers, the wide ones are busbars, and the patches are PAD points. Only one of those three is a printing decision. The other two exist because something has to be soldered to the cell.

That is the part of the 0BB story that gets compressed into a single sentence about silver paste. Removing the busbar does cut silver, and the number is large enough to matter. But the busbar also carried a mechanical job: it was the flat, wide, tolerant surface that a ribbon could be soldered onto, and the metal edge that told the stringer where the ribbon belonged. Take it away and both jobs have to be rebuilt out of something else.

What follows is the cell-side and line-side view of that rebuild. If you want the back-contact version, where both polarities sit on the rear and the wire routing has to change before the wire count does, that is a separate article: 0BB on back-contact cells.

Side by side diagram of a conventional solar cell front carrying busbars, fingers and PAD points, and a 0BB cell front where many thin wires bond directly to the fingers with no busbar or PAD

What the busbar actually does

Three jobs, and only the first one is electrical.

The first is collection. A finger is deliberately thin because every micrometre of front metal shades the cell, and thin metal is resistive. A finger cannot carry its current all the way to the edge of the cell without losing a measurable share of it, so it hands the current to a much wider conductor running perpendicular to it. That is the busbar: low resistance, short path, one junction per finger.

The second is landing. Solder needs area. A joint is only as strong as the metal it is formed on, and a ribbon soldered onto a finger-width line would have almost no peel strength. The busbar is where the ribbon lands, and the PAD is the thickened patch inside it that carries the joint and distributes the mechanical load of a ribbon that expands and contracts with temperature.

The third is location. During stringing, the ribbon has to be placed within a fraction of a millimetre. The busbar is what the machine and the operator align to: a visible metal band of known width, sitting under the ribbon. It tolerates small offsets because it is far wider than the ribbon. This is the job that gets forgotten in discussions of silver reduction, and it is the one that has to be replaced by a consumable or a process step.

Three panel diagram showing the busbar collecting current from many fingers, providing a wide PAD for the ribbon to be soldered onto, and acting as the placement reference that locates the ribbon during stringing

What 0BB removes, and what it does not

Zero busbar means exactly that: the printed busbar is gone, and with it the PAD cluster that sat on top of it. The fingers stay. They have to: they are what collects the current from the silicon, and no interconnection scheme removes them.

What arrives in their place is a set of very thin round wires, typically more than twenty of them across the cell, running the same direction the busbars used to run. Each wire crosses the fingers rather than collecting at one point, and each crossing is a joint. One cell that used to have a handful of large soldered joints now has several hundred small ones.

Several consequences follow from that single substitution, and they show up in different places:

  • Shading falls, because twenty thin wires cover less area than three or four wide busbars, and round wire reflects part of the light it intercepts back into the glass.
  • Series resistance falls, because the current in each wire is a small fraction of the cell current and the path length is shorter than the route through a busbar and along a ribbon.
  • Cell silver falls, because the widest printed features are the ones being deleted. See the arithmetic below.
  • Joint area falls, by roughly an order of magnitude per joint, which is where the process difficulty comes from.
  • Placement tolerance tightens, because a wire that lands between fingers on a busbarless cell has no wide metal to fall back on.

The silver arithmetic, and where the saving really goes

Busbars are wide and there are only a few of them; fingers are narrow and there are a hundred or more. That comparison alone does not settle the silver question, so it is worth putting the two features side by side in the terms a printing engineer would use.

Printed featureTypical printed widthWhat 0BB does to it
FingerTens of micrometresStays, and may be widened slightly at the bonding points
BusbarAround half a millimetre and upDeleted
PADLarger than the busbar widthDeleted with the busbar, unless a hybrid process rebuilds it
Interconnect metalRibbon, silver-bearing coating on copperReplaced by bare copper wire, plus a film or an adhesive

A busbar is roughly fifteen to thirty times wider than a finger. There are far fewer of them, so the comparison is not overwhelming. The busbar plus PAD cluster is still a real share of the cell's printed silver, and it is concentrated on the feature that is easiest to delete, because it does no collecting.

Published estimates for how much cell silver disappears with the busbars sit in a wide band, from roughly a fifth to roughly two fifths, and the spread is not noise. It depends on how many busbars the cell had, how the fingers are redesigned afterwards, and which paste system is in use. A low-temperature paste cell with many busbars has more busbar silver to remove than a high-temperature cell with five, which is why the saving is usually described as largest on heterojunction platforms. Treat the range as an orientation figure quoted in the trade press rather than a specification.

The other half of the arithmetic is where the money goes instead. The wire itself is copper, which is far cheaper than silver. The route that holds it is not free, though: a foil or a film is a purchased material with its own yield, adhesive is a consumable, and the dispenser, the curing station or the welding capability is equipment. A line that saves silver paste and buys film has moved cost rather than deleted it, and the trade only works if the cell-side saving exceeds the consumable bill per watt. This is the same system-level calculation that governs every other silver reduction route, and it is worth reading alongside our comparison of copper paste, copper plating and less-silver paste.

Four ways to connect a busbarless cell

Every route on the market answers the same question: what holds each wire in contact with its finger until a permanent joint exists. They differ in whether that answer is a purchased material or a process step.

RouteWhat holds the wireWhat it adds to the line
Multi-wire foilWires pre-embedded in a polymer foilA foil supply and a placement step; the joint forms in the laminator
Film (skin film)A film laid over wires and cell and hot-pressedFilm material, a pressing step, and an extra layer in the stack
Adhesive dispensingUV or hot-melt dots at fixed pointsDispenser, curing, and adhesive as a consumable
Weld plus adhesiveA local weld on a widened finger, reinforced by adhesiveA modified finger design and welding capability

The first two are materials decisions, the last two are process decisions, and the practical difference is where the joint is completed. In the foil and film routes, the wire is held mechanically and the electrical contact is completed during lamination, when heat and pressure press the wire into the finger. In the dispensing route the adhesive pins the wire at defined points and the alloy contact again forms in the laminator. In the weld-plus-adhesive route, part of the joint is made on the stringer, immediately, and the adhesive is there to stop the wire moving afterwards.

Four panel diagram comparing how 0BB cells are interconnected: wires embedded in a polymer foil, a film pressed over wires and cell, adhesive dots pinning each wire, and local welds on widened finger pads reinforced with adhesive

A note on the foil route: it is tied to a specific licensor rather than being openly available, which is why it appears in fewer lines than its electrical performance alone would predict. The film, adhesive and hybrid routes are the ones most commonly adopted by manufacturers building or converting a line, and they are described below in the terms that matter on the floor.

What each route does to the line

Once the wire is on the cell, the next question is what happens when the joint is bad. That question has different answers depending on the route, and the answers have a price.

Electroluminescence is how a hidden joint defect is normally found: a cell that is not properly connected shows up as a dark region under forward bias. In a film or dispensing route, however, the wire is only pressed against the finger by the film or the adhesive, and the electrical contact that EL would reveal is completed later, inside the laminator. Before lamination there is nothing to image at that interface, so the first meaningful inspection point is after the module is built.

The hybrid route changes that. Because the weld is made on the stringer, a string can be inspected immediately, before layup, while it is still possible to pull a bad string and rework it instead of scrapping a laminated module. For a process with hundreds of small joints per cell, that difference is not a detail. A defect rate that would be negligible with three joints per cell becomes material with three hundred, and the cost of finding it after lamination is the cost of the whole module, not of the string.

Timeline of stringing, pre-lamination electroluminescence, layup, lamination and post-lamination electroluminescence, showing that film and adhesive dispensing routes can only be inspected after lamination while the weld plus adhesive route allows inspection before layup

The rest of the comparison is a list of trades rather than a ranking. The film route holds the wire firmly and leaves no flux residue to clean, at the cost of a purchased film and an extra layer in the stack. Dispensing uses less material and is the easiest to retrofit onto an existing line, but the bond between wire and cell relies on the adhesive and the lamination cycle, and it is the route most likely to need extra reliability testing before it is trusted. The hybrid route produces the strongest bond and the earliest inspection window, and pays for it with a more demanding finger design, welding heat that can shrink a thin wire, and an additional consumable.

One constraint applies to all four: the wire has to be placed accurately. On a busbar cell, a ribbon offset by a fraction of a millimetre still lands on metal. On a busbarless cell, the same offset can put a wire in the gap between two fingers, where it contributes nothing. That turns placement accuracy from a quality target into a yield driver. It is one of the reasons the machine side of 0BB has moved as fast as the cell side. Our guide to tabber and stringer machines covers what those machines are asked to hold, and the SS-2500B stringer is an example of a platform specified up to 20BB.

Where the risk sits

0BB does not fail for electrical reasons. The current path is better than the one it replaces, and that is why the architecture spread. It fails, when it fails, at the joint and at the handling around it.

Peel strength is the first number to watch, and it moves in the wrong direction by construction. A joint's strength comes from its bonded area, and 0BB shrinks that area by roughly an order of magnitude per joint. What remains is a very large number of very small bonds, each one individually weak. This is survivable, because load sharing across hundreds of joints is not the same as load concentration on three. It does change what a peel test means, though: the average matters less than the spread, and the weakest joint in a string is what handling and lamination will find.

Handling is the second exposure. Busbarless cells have less stiff metal to resist bending, and the connecting wires are fine enough to be damaged by a rough transfer. Thin wafers that were already at the edge of what a stringer could carry are the ones where 0BB is most attractive and least forgiving. This is why the metrology that matters most on a 0BB line is not power measurement but electroluminescence, and it is worth running it at more than one point in the flow, a point our inline and offline EL comparison covers in detail.

The third exposure is the consumable itself. A film is an extra layer in the stack, which means an extra interface to qualify for damp heat and an extra source of optical loss if its transmission is not what the datasheet promised. An adhesive adds a polymer at the joint, and the long-term question is not whether it holds on day one but whether it holds after humidity and thermal cycling. A weld adds local heat to a thin wafer and can shrink the wire it is welding, which is why the hybrid route is paired with an adhesive rather than trusted alone.

None of these are reasons to avoid 0BB. They are the reason the qualification programme for a 0BB line looks different from the one for a busbar line: fewer samples of power, more samples of joints, and a reliability sequence that stresses the interface rather than the wafer.

Choosing a route: five questions

The route is not chosen on cell efficiency. It is chosen on what the line already has, what a defective joint costs, and what the customer's reliability expectation is. Five questions sort most of it out.

QuestionWhy it decides the route
What does a scrapped module cost you?If it is high, the earliest possible inspection window is worth paying for, which favours the welded hybrid route
Is the line new or converted?Dispensing is the smallest change to an existing stringer; film and foil routes want a placement step and a stack that accommodates them
Can you redesign the cell metallisation?The hybrid route needs widened fingers at the bonding points; the other routes work with a conventional finger layout
What residue is acceptable?Flux-bearing welding needs a cleaning or a no-clean chemistry decision; film and adhesive routes avoid it, which matters on the film side of a bifacial module
Which reliability test will your customer quote?Joint-level degradation in damp heat and thermal cycling is the usual failure, so the route with the most accumulated field data carries a commercial advantage

If the answer to the first question is "a great deal", the inspection window matters more than the consumable bill. If the answer to the second is "we are converting the line we have", the adhesive route wins almost by default. There is no route that is best on all five axes, which is why lines in the same market run different ones.

Frequently asked questions

Does 0BB mean there is no metal printed on the front of the cell?

No. The fingers stay, and they still cover the front surface in fine parallel lines. What disappears is the busbar and the PAD cluster: the wide conductors that the fingers used to feed and the ribbon used to be soldered onto.

If the wires are copper, why does the cell's silver consumption fall?

Because the silver that is removed was never doing any collecting. The busbar and PAD are wide printed features whose job was to be a landing zone and a low-resistance collector. Removing them removes silver; the wires that replace them are copper and are bought from a different supplier at a very different price. What does not change is the finger silver, which is the majority of the printed metal on most cells.

Which of the four routes is best?

There is no single answer, and anyone who gives one is describing their own line. The foil route performs well and is tied to a licensor. The film route gives a firm bond and no flux residue at the cost of a purchased material. Dispensing is the cheapest to adopt and the least proven on joint strength. The welded hybrid gives the strongest joint and the earliest inspection, and asks the most of the cell design and the machine.

Can an existing busbar stringer be converted?

Usually yes, but not equally across routes. Adding a dispenser and a curing step is the smallest change. A film or foil route needs a placement step and enough stack height for the extra layer. A welded hybrid needs the cell's fingers redesigned and a machine that can weld a very thin wire without damaging the wafer. All of them need placement accuracy better than a busbar line needed, because there is no wide metal to absorb an offset.

Does 0BB work with every cell technology?

It has been applied across the mainstream ones, and the incentive is largest where the paste is expensive and the busbar count is high, which points at heterojunction. Back-contact cells add a separate constraint: both polarities sit on the rear, so wires must not bridge lanes of opposite polarity, which changes the routing before it changes anything else. Our back-contact cell explainer covers that layout in detail.

What fails first on a 0BB module?

In most reported sequences, the joint rather than the cell: joints that lose strength after temperature cycling, or wires that move during handling because the only thing holding them was a film or an adhesive that had not yet been through lamination. Cracks in thin wafers follow, especially where handling is not adapted. Power loss from the interconnection itself is the one failure mode that becomes less likely rather than more.

Final thoughts

The useful way to think about 0BB is as a transfer of responsibility. The busbar used to collect the current, provide a solderable pad and establish where the ribbon goes. Deleting it hands collection to the wires, and hands the other two jobs to a material or a machine setting: a film that must be purchased, an adhesive that must be cured, a weld that must be timed, a finger that must be widened.

That is why two lines can both run 0BB and have almost nothing in common operationally. The cell looks identical at the front. The differences live in the stack, in the consumable bill, in where the electroluminescence camera sits, and in how much a scrapped module costs when a joint goes wrong. Choose the route on those four things and the silver saving takes care of itself; choose it on the silver saving alone and the first bad lamination batch will explain the rest.

Related reading

0BB on back-contact cells: gains and yield limits · What a PV ribbon does: three jobs, one trade-off · PV ribbon structure and types · PV ribbon materials: copper core, hardness and coating · Stringer market and technology report: 0BB trends · Tabber and stringer machines · From cell to module: the manufacturing process · No-clean flux for n-type cell soldering · PV cell metallization and the copper question · Solar panel manufacturing stations and line layout

The numbers in this article are our own arithmetic or descriptions of typical geometry, not measured product data, and no manufacturer test results are quoted. The width comparison treats a printed busbar as roughly 0.5 mm and up against fingers printed in the tens of micrometres, which is a typical range rather than a specification. The 20 to 40 percent figure for cell-level silver reduction when busbars are removed is a range widely quoted in the trade press, not a measurement of ours; it varies with the number of busbars, the paste system and how the finger layout is redesigned afterwards. A 20-wire cell crossing around a hundred fingers has on the order of a thousand wire-to-finger crossings, and we describe the resulting joint count as several hundred to stay conservative, since not every crossing becomes a bonded joint in every route. Actual results depend on the cell design, the interconnection route and the process window.

Flat vs round ribbon: why BC cells break the rule — why the busbar was there at all, and what replaces it

Tags :

Request A Quote

All uploads are secure and confidential.

Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

OPT-M960B EL & VI Tester: 0.1mm/pixel, Intel i7
2025-09-06 11:38:03

OPT-M960B EL & VI Tester: 0.1mm/pixel, Intel i7

Ooitech offers professional solar panel EL tester and VI tester machines (OPT-M960B, OPT-M951B, OPT-M950B) with SONY industrial cameras

Read More
Solar Panel Manufacturing Machine: A Station-by-Station Guide
2026-10-29 12:48:41

Solar Panel Manufacturing Machine: A Station-by-Station Guide

Station-by-station guide to each solar panel manufacturing machine: cell cutting, tabbing, layup, bussing, lamination, framing, testing.

Read More
IEC 61215 & 61730 Test Equipment: 0.1-10kV, 2600mm
2025-09-08 14:12:26

IEC 61215 & 61730 Test Equipment: 0.1-10kV, 2600mm

Ooitech offers a complete range of solar panel testing equipment for IEC61215 and IEC61730 certification, including visual inspection stations

Read More
BC Cell Tabber Stringer: 1000 Cells/h for IBC, ABC, HPBC
2025-08-17 17:41:21

BC Cell Tabber Stringer: 1000 Cells/h for IBC, ABC, HPBC

A BC cell tabber stringer welds IBC, ABC and HPBC cells on the rear face: 0.2 mm placement, 1000 cells/h, 0.2% breakage on Class A wafers.

Read More
EVA Encapsulant Film: 80 N/cm Peel, EVA vs POE vs EPE
2025-09-08 14:22:26

EVA Encapsulant Film: 80 N/cm Peel, EVA vs POE vs EPE

EVA encapsulant film for solar modules, plus POE and EPE options: anti-PID, UV-resistant and compatible with TOPCon and PERC lines, in your thickness.

Read More
Solar Panel Sealant and Tape: Silicone, Butyl, PET
2025-09-09 17:18:55

Solar Panel Sealant and Tape: Silicone, Butyl, PET

Solar panel sealant and tape for module assembly: silicone frame sealant, butyl tape and busbar insulation tape, UV-resistant for 25-year outdoor exposure.

Read More
AI research shortcut

Ask AI About OOITech

One click opens your AI assistant with a question about our solar panel production lines already filled in — the turnkey PV module lines we build, from semi-automatic to GW-scale, and what a quote needs.

Get a Quote