Follow Us:
Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules
  • 2026-07-20
  • 205 Views
  • Blog

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Product Introduction

Center hole cracks are the most frequent cosmetic defect you run into on a PV module line. The causes are messy and there are a lot of them. This post narrows things down and looks only at the center hole cracks that come from problems in the bussing (overlap soldering) step. Three typical root causes, walked through one at a time.

Technical Parameters
Reserved gap between ribbon and cell edge is too small

The cell edge sits too close to the bus bar.

TOPCon cell strings use a front-side ribbon positive structure, and the ribbon is soldered to the back of the bus bar. During bussing the machine does bring the cell and bus bar to the same plane, but the two materials differ a lot in thickness:

ItemThickness
Standard TOPCon wafer0.13mm
Middle bus bar0.35mm~0.4mm

Once you get into lamination, the contact area where the ribbon meets the cell edge sees a two-way force.

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

When the gap between cell and bus bar is too small, the angle between the ribbon and the wafer edge shrinks. Pull force F1 drops, and vertical pressure F2 goes up at the same time.

Wafers are brittle. Under that higher pressure the edge cracks easily, and you end up with a center hole crack.

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Technical Advantages
Ribbon bends and deforms after forming

If the plane difference between cell and bus bar is too large during bussing, the ribbon keeps a height difference after it's soldered.

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Bussing has already fixed the total ribbon length. The extra length has nowhere to go, so the ribbon bends to absorb it. That bent ribbon then keeps pressing on the cell edge, and you get batch center hole cracks.

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Solder ring defect during bussing (a rarer batch cause)

Here the cell and bus bar have a slight plane difference during bussing, and the harpoon area has no bus bar support, so the ribbon separates from the wafer. When the solder heat melts the ribbon coating, a raised ring of solder forms around it. During lamination pressure this hard solder ring pushes straight into the wafer and cracks it, giving another center hole crack.

Why Bussing (Overlap Soldering) Causes Cell Cracks During Lamination in PV Modules

Product Application

These three failure modes show up across most crystalline module lines, and they matter most on thin, high-efficiency cells where the mechanical margin is already tight. Watching ribbon-to-cell spacing, plane alignment during bussing, and solder profile control gives you the biggest lever on center hole crack yield.

Ooitech's View

Thin TOPCon wafers at 0.13mm leave almost no room for error, so the F1/F2 force balance we talk about here is really an alignment problem you solve upstream at the stringer and bussing stations, not something you can fix later in lamination. On the module lines we build, keeping the cell and bus bar coplanar and holding a steady solder profile is where most center-crack yield actually comes from. If you want to see how these steps run in a real factory, Ooitech's YouTube channel www.youtube.com/ooitech has plenty of line footage worth a look.


Tags :

Request A Quote

All uploads are secure and confidential.

Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

Automatic Layup & Bussing Integrated Machine SAW-100A | Solar Panel Production Equipment | Ooitech
2025-09-05 22:36:46

Automatic Layup & Bussing Integrated Machine SAW-100A | Solar Panel Production Equipment | Ooitech

Ooitech SAW-100A Automatic Layup & Bussing Integrated Machine delivers high-efficiency cell string layup and terminal busbar welding with high frequency electromagnetic soldering, mechanical and fiber optic positioning, and capacity up to 15S per grou

Read More
SC-20D Dual-Laser Solar Cell Cutting Machine for Shingled Solar Cell Production
2025-08-17 17:41:21

SC-20D Dual-Laser Solar Cell Cutting Machine for Shingled Solar Cell Production

SC-20D is the advanced version of SC-20A, specially designed for shingled solar cell production, featuring dual laser heads and two lasers working simultaneously for higher-throughput cutting.

Read More
OSLB-1300 Back Contact Cell Welding Machine | BC Solar Cell Stringer for IBC ABC HPBC Panel Production
2025-08-17 17:41:21

OSLB-1300 Back Contact Cell Welding Machine | BC Solar Cell Stringer for IBC ABC HPBC Panel Production

OSLB-1300 back contact cell welding machine by Ooitech delivers ≥1000 cells/hour throughput for BC, IBC, ABC, and HPBC solar cell string welding. Features A/B dual cell loading, CCD + SCARA robot positioning (±0.2mm), infrared heating welding, inline EL i

Read More
Junction Box Welding Machine KS-01C | Automatic Solar Panel Junction Box Soldering Equipment - Ooitech
2025-09-06 13:27:54

Junction Box Welding Machine KS-01C | Automatic Solar Panel Junction Box Soldering Equipment - Ooitech

Ooitech KS-01C Junction Box Welding Machine features automatic hot bar tin welding and high frequency welding with CCD positioning accuracy of ±0.1mm. Supports 5BB-12BB full cell, half-cut, and bifacial modules. Cycle time ≤16s with 99.6% welding quality

Read More
C350-CQC EVA, TPT, and PPE strips Cutting &Punching Machine – Solar Busbar Processing
2025-09-08 14:44:14

C350-CQC EVA, TPT, and PPE strips Cutting &Punching Machine – Solar Busbar Processing

C350-CQC punching & cutting machine – 30 pcs/min, ±0.2mm accuracy for EVA, TPT & PPE solar materials. Precision processing for busbar and encapsulant components in PV production lines.

Read More
SS-1500B Automatic Solar Cell Welding Machine - High-Speed Tabber Stringer for BC/TOPCON/PERC Cells
2025-08-17 17:41:21

SS-1500B Automatic Solar Cell Welding Machine - High-Speed Tabber Stringer for BC/TOPCON/PERC Cells

SS-1500B automatic solar cell welding machine by Ooitech - High-performance tabber stringer for BC, TOPCON, PERC, and HJT cells with 1000-1200 PCS/H capacity, CCD+robot positioning system, infrared welding technology, and integrated EL inspection for effi

Read More