Solar Anodizing: Why Frames Use Anodized Aluminum
  • Jerry
  • 2026-06-24
  • 981 Views
  • Blog

Editorial responsibility for this article rests with Wuhan Ooi Photoelectric Technology Co., Ltd. Written and reviewed by the Ooitech editorial team. See our editorial policy for how we write, where AI tools are used, and how to request a correction.

Solar Anodizing: Why Frames Use Anodized Aluminum

Quick answer: Anodising is the mainstream surface treatment for solar module aluminium frames because it grows an oxide layer out of the aluminium itself rather than applying a coating on top of it. That matters for a component expected to survive 25 years outdoors: a paint or powder coat can chip and let corrosion start at the exposed edge, while an anodised layer is integral to the surface. Thickness is specified by anodising class, and standards such as CPIA 0117 define classes AA10, AA15 and AA20, with the number denoting the oxide thickness in microns. Thicker anodising gives more corrosion margin and costs more. Frame alloy selection interacts with this — a 6063 extrusion with a defined temper such as HV300 behaves predictably through anodising, where a poorly controlled alloy can produce a patchy finish and a weaker oxide layer.

PV Module Manufacturing · by Jerry, Ooitech

Introduction

In a PV module, the aluminum frame works as the key sealing and structural material. Its cost share sits right behind the solar cells, usually between 8.5% and 13%, making it one of the core parts that keeps a module running reliably outdoors for 25 years or more.

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

There are several ways to treat the surface of an aluminum frame, including anodizing, electrophoretic painting, and powder coating (PVDF). But anodizing (especially silver-white and black) has become the absolute mainstream choice. This isn't by chance. It's because anodizing can systematically and comprehensively meet the strict performance demands a PV module places on its frame. The core reasons can be grouped into the following points.

Building a Superior Corrosion Barrier for Harsh Environments

PV modules have to serve for the long haul under all kinds of climates worldwide, from dry deserts and humid rainforests to highly corrosive coastal, offshore, and industrial zones. These different conditions put tough weathering requirements on the frame. The aluminum frame must withstand UV radiation, day-night temperature swings, acid-alkali-salt spray, and sand abrasion. Aluminum does form a natural oxide layer in air, but it's thin (about 0.1μm), uneven, and porous. In such environments that natural layer is about as protective as a sheet of paper.

Anodizing uses an electrochemical method to grow a dense, hard, and strongly bonded aluminum oxide (Al₂O₃) ceramic film in-situ on the aluminum alloy surface. This artificially enhanced layer is the foundation of the frame's corrosion resistance.

The anodic film thickness standard for PV aluminum frames sits between 10 and 25μm. This range is set with several factors in mind: enough film thickness effectively isolates the aluminum substrate from the outside environment, blocking moisture, salt spray, and acid rain from corroding the frame, which extends the module's service life under harsh outdoor weather.

If the film is too thin (say, below 10μm), the frame's protection may fall short, leading to local breakdown of the oxide film and triggering pitting or cracks that affect overall structural strength. On the other hand, if the film is too thick (over 25μm), protection improves but production cost rises, and an overly thick layer is more brittle, making it more prone to cracking under impact during installation or transport, which actually lowers reliability.

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

Under the standard T/CPIA 0117-2025, anodic films are graded by thickness (such as AA10, AA15, AA20) to match different corrosion environments. For example, the AA15 grade is recommended for more corrosive settings like industrial parks and chemical plants, while AA20 is reserved for very high corrosion environments such as coastal areas and mines.

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

Delivering the Right Conductivity and Grounding Safety While Keeping Insulation

This is a seemingly contradictory but crucial property. Aluminum is a good conductor, which lets the frame easily serve as part of the module's grounding path, channeling lightning current or static to deliver lightning protection and grounding continuity for system safety.

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

Yet the anodic film itself is an excellent electrical insulator. This insulating layer first protects the frame body, preventing it from becoming the anode of electrolytic corrosion in damp conditions. Second, it isolates the frame from mounting brackets and other metal parts (especially metals at different potentials, like steel bolts), greatly easing the galvanic corrosion that dissimilar-metal contact can cause. Failure cases in offshore PV show that aluminum alloy frames and steel bolts suffer serious electrochemical corrosion in salt-spray environments, and a thicker anodic film (combined with insulation-coated bolts) is one of the key processes that solves this problem.

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

PS: Grounding a PV module really matters. As the person who handled a customer complaint where a lightning strike blew out a junction-box diode, when I got to the site I found the installer had taken no grounding measures at all on the module (no use of frame grounding holes, piercing washers, or piercing screws).

Enhancing Mechanical Performance and Wear Resistance to Protect Structural Integrity

The frame needs to bear loads such as wind pressure, snow load, and mechanical impact that the module meets during transport, installation, and operation.

High hardness and wear resistance: The anodic film has very high hardness (typically above HV300), far higher than the aluminum substrate. This boosts the frame surface's scratch and wear resistance, better protecting itself during installation and maintenance and reducing corrosion start points and loss of appearance caused by surface damage.

Strong adhesion: The anodic film grows directly out of the aluminum base through a chemical reaction and bonds as one with the substrate, with none of the peeling or flaking risk seen in sprayed coatings. This very strong adhesion ensures lasting protection, and even after long-term thermal expansion and contraction the film won't fall off.

Supporting long-life design: Aluminum alloy material itself can last 30 to 50 years. Anodizing further safeguards structural integrity and strength stability across the whole PV module life cycle (usually 25 years or more). By comparison, frames made of other materials, such as steel frames, easily rust at grounding holes and other spots, making a 25-year life hard to guarantee, while the long-term reliability of composite-material frames is still being verified.

太阳能伏边框_安徽鑫铂科技有限司

A Mature Process and Complete Standard System That Ensure Quality and Supply

Anodizing is an extremely mature and standard surface treatment in the aluminum processing industry, with a complete supply chain, high processing efficiency, and relatively controllable cost. Multiple brokerage reports note that the aluminum frame manufacturing process (melting and casting - extrusion - oxidation - deep processing) is very mature, which is the basis for its over-95% penetration in the PV field.

Why Anodizing Is the Mainstream Surface Treatment for Solar Frames

Aluminum frames offer mature standardization and controllable quality. From national standards (such as GB/T 5237.2) to PV association group standards (T/CPIA 0117), there are clear and testable indicators for the anodic film's thickness, hardness, sealing quality, and salt-spray resistance. This gives quality control a solid basis and ensures product consistency and reliability.

In the framing step, the frame needs to be bonded and sealed to the glass and backsheet with sealant. The anodized surface has a certain micro-porous structure that forms good adhesion with the sealant, ensuring reliable module sealing.

QQ截图20171030163707

In the end, choosing anodizing for the PV aluminum frame is an "optimal solution" verified through long-term industry practice.

Ooitech's View

Ooitech believes: anodizing has become the mainstream surface treatment for PV aluminum frames because it simultaneously satisfies corrosion resistance, grounding safety, mechanical strength, and standardized quality control over a module's 25-year-plus service life.

Further reading and background data

Public reference material on this topic, published by the organisations that maintain the industry's technology roadmap and market data:


Tags :

Request A Quote

All uploads are secure and confidential.

Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

EVA Encapsulant Film: 80 N/cm Peel, EVA vs POE vs EPE
2025-09-08 14:22:26

EVA Encapsulant Film: 80 N/cm Peel, EVA vs POE vs EPE

EVA encapsulant film for solar modules, plus POE and EPE options: anti-PID, UV-resistant and compatible with TOPCon and PERC lines, in your thickness.

Read More
SL-1000 Back Contact Cell Welder: 600 Cells/h
2025-09-05 21:43:58

SL-1000 Back Contact Cell Welder: 600 Cells/h

SUNPOWER Back Contact Cell Welding Machine SL-1000 by Ooitech features electromagnetic welding, CCD+SCARA robot positioning, dual cell loading

Read More
Solar Tempered Glass: 93.5% Transmittance, Low-Iron
2025-09-08 14:17:29

Solar Tempered Glass: 93.5% Transmittance, Low-Iron

Solar tempered glass for PV modules: ultra-clear low-iron glass with anti-reflective coating, reaching 91.5%+ light transmittance in G1/M6/M10/M12 sizes.

Read More
ST-TLD3A+ IV Tester – PV Module Flash & Performance
2025-09-08 14:05:49

ST-TLD3A+ IV Tester – PV Module Flash & Performance

ST-TLD3A+ / SMTL-V21.3A+ solar IV tester – A+ spectrum, tests mono, poly, TOPCon, HJT, IBC & thin film. Accurate I-V/P-V curves for full module

Read More
Automatic Layout & Bussing Integrated Machine
2026-03-24 17:53:42

Automatic Layout & Bussing Integrated Machine

Ooitech ALU-HBL Automatic Layout & Bussing Integrated Machine combines cell string positioning, layout, and electromagnetic busbar welding in one

Read More
BD03 Frame Gluing Machine: 3-4s per Meter, 2500mm
2025-09-06 13:42:28

BD03 Frame Gluing Machine: 3-4s per Meter, 2500mm

BD03 CNC frame gluing machine – automated aluminum frame sealant application with precise positioning, automatic feeding and uniform glue distribution for

Read More
AI research shortcut

Ask AI About OOITech

One click opens your AI assistant with a question about our solar panel production lines already filled in — the turnkey PV module lines we build, from semi-automatic to GW-scale, and what a quote needs.

Get a Quote