Breakthrough in Semi-Transparent Organic Solar Cells: High Thickness Tolerance Enables BIPV Revolution
  • 2026-04-22
  • 104 Views
  • Blog

Breakthrough in Semi-Transparent Organic Solar Cells: High Thickness Tolerance Enables BIPV Revolution

Introduction

Building-Integrated Photovoltaics (BIPV) has emerged as a critical pathway for urban sustainable energy transition. Among various technologies, semi-transparent organic solar cells (ST-OSCs) stand out as ideal candidates for self-powered windows due to their tunable bandgap and intrinsic semi-transparency. However, conventional ST-OSCs face a major bottleneck: to balance transparency and efficiency, the active layer must remain extremely thin (below 80 nm), which creates severe challenges for large-scale industrial manufacturing. Tiny thickness fluctuations can cause dramatic performance drops, and the cell-to-module (CTM) efficiency retention for large-area modules typically stays below 56%.

A recent breakthrough published in Nature Communications by teams from the National Center for Nanoscience and Technology (NCNST) and collaborators addresses this long-standing issue. By combining a donor dilution strategy with slot-die coating under halogen-free solvent conditions, the researchers successfully fabricated ST-OSCs with remarkable thickness tolerance. Even with an ultra-thick 301 nm active layer, the devices maintained high light utilization efficiency (LUE), and 100 cm² modules achieved a CTM ratio of approximately 85%.

Research overview

Performance Leap in Light Utilization Efficiency

In BIPV applications, semi-transparent cells have long faced a fundamental trade-off: increasing active layer thickness improves photon absorption and power conversion efficiency (PCE), but significantly reduces average visible transmittance (AVT). The industry evaluates ST-OSCs using Light Utilization Efficiency (LUE = PCE × AVT) as the key metric.

This study introduces a donor dilution strategy with a D:A ratio of 1:3, leveraging the fibrous network structure of acceptor materials under specific processing conditions. This approach allows substantial increases in active layer thickness while maintaining high transparency.

The observed data is striking. When the active layer thickness increased from 119 nm to 301 nm, the PM6:Qx-p-4Cl based cells maintained an LUE of 3.02%, demonstrating exceptional thickness robustness. This solves a critical pain point in large-area processing where thin film control has been notoriously difficult.

Device characteristics and logic framework

Figure 1 shows the chemical structures and absorption spectra of PM6:Qx-p-4Cl system, performance trends across different D:A ratios for opaque and semi-transparent devices, and demonstrates how the donor-diluted system outperforms conventional systems in transmittance retention and LUE advantage across varying thicknesses.

Mechanism Behind Thickness Tolerance

Why does the donor dilution approach solve the thickness sensitivity problem? The research team conducted thorough investigations through morphology studies and ultrafast spectroscopy.

Regarding morphological features, slot-die coating under specific conditions promotes ideal aggregation of acceptor molecules, forming continuous interpenetrating fibril-like networks. This structure ensures smooth charge transport even when donor content is extremely low.

For exciton dynamics, experimental measurements revealed that the Qx-p-4Cl acceptor possesses a remarkably long exciton diffusion length of approximately 22.34 nm. This ensures that excitons can effectively reach interfaces and dissociate even in thick, diluted systems.

Charge generation analysis via transient absorption (TA) spectroscopy confirmed that the system maintains efficient and stable charge generation across different thicknesses and ratios.

Morphology and photophysical characterization

Figure 2 presents GIWAXS and AFM characterization revealing the fibril network structure, alongside transient absorption spectra and kinetic curves demonstrating robust charge generation and transport in the donor-diluted system.

Film Formation Dynamics: Slot-Die vs Spin Coating

The research further uncovered the physical essence of why slot-die coating outperforms traditional spin coating processes.

Unlike spin coating where films undergo burst-like aggregation in supersaturated states, slot-die coating on heated substrates induces orderly acceptor aggregation already in the liquid phase. This fundamentally changes the morphology evolution pathway.

Viscosity control plays a crucial role as well. Donor dilution reduces solution viscosity, accelerating solvent evaporation and extending the crystallization time after film thinning. This suppresses excessive acceptor aggregation at large thicknesses.

This unique film formation dynamic ensures that during large-area coating, film quality remains less sensitive to process parameter fluctuations, a critical factor for industrial production consistency.

In-situ film formation analysis

Figure 3 shows in-situ UV-Vis absorption spectroscopy monitoring the acceptor aggregation process, along with comparative schematics of film formation mechanisms under spin coating versus slot-die coating, highlighting the critical regulatory role of heated substrates on morphology evolution.

Industrial Prospects and BIPV Applications

Leveraging the processing advantages from high thickness tolerance, the research team successfully translated the technology into practical applications.

On 100 cm² modules, they achieved 10.40% PCE and 3.32% LUE with a CTM ratio reaching 85%, setting a new benchmark for large semi-transparent modules.

For BIPV function demonstration, the team built a self-powered house model with a 600 cm² power-generating window. Experiments proved the system could drive LCD displays and charge lithium batteries.

The energy-saving benefits are equally impressive. Because the active layer blocks 88.28% of near-infrared radiation, the cell windows reduced indoor temperatures by approximately 9.2°C compared to ordinary glass windows, significantly cutting building energy consumption.

Stability testing showed that after 1000 hours of outdoor exposure, devices retained over 82% of their initial efficiency, demonstrating excellent commercialization potential.

Module performance and BIPV field testing

Figure 4 displays the 100 cm² module structure and CTM efficiency statistics, along with BIPV application demonstrations including self-powered electronic device operation, energy storage, and the significant thermal insulation cooling effect curves.

Conclusion and Outlook

This research provides critical support for organic photovoltaics in green building and energy internet applications through several key contributions.

First, it lowers manufacturing barriers by breaking the dependence of ST-OSCs on ultra-thin films. High thickness tolerance translates directly into higher production yields and lower costs.

Second, it enables multi-dimensional carbon reduction. ST-OSC windows contribute green electricity through photovoltaic generation while simultaneously reducing building air conditioning passive energy consumption through excellent thermal insulation.

Third, the technology demonstrates broad applicability. The donor dilution strategy combined with halogen-free solvent processing aligns with green manufacturing trends, clearing obstacles for organic photovoltaics to move toward industrial-scale production lines.

As the world advances toward carbon neutrality, this smart energy solution integrating power generation, energy saving, and aesthetic appeal is transforming every building into a micro green power plant.

Original article: https://www.nature.com/articles/s41467-026-69537-3

Ooitech Perspective

Ooitech believes: donor dilution combined with slot-die coating breaks the thickness tolerance bottleneck of semi-transparent organic solar cells, paving a realistic path for BIPV industrialization and large-area commercial deployment.



Tags :

Request A Quote

All uploads are secure and confidential.

Why Choose Us

We deliver expertise you can trust our service

Direct-from-Factory Equipment.

Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

Testimonials

What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. Know More

Our Products

Our Latest Products

Junction Box AB Component Filling Glue Machine SPZ-AB10S-JH | Ooitech Solar Panel Production Equipment
2025-09-06 13:34:54

Junction Box AB Component Filling Glue Machine SPZ-AB10S-JH | Ooitech Solar Panel Production Equipment

Ooitech SPZ-AB10S-JH Junction Box AB Component Filling Glue Machine delivers precise two-component adhesive mixing and dispensing for solar panel junction boxes. Features screw and gear metering system with ±2% proportion accuracy, PLC and HMI control, an

Read More
EVA/POE/EPE Encapsulant Film – Solar Cell Bonding & Protection
2025-09-08 14:22:26

EVA/POE/EPE Encapsulant Film – Solar Cell Bonding & Protection

EVA, POE & EPE encapsulant films for solar module production – anti-PID, UV-resistant, compatible with TOPCon, HJT & bifacial modules. Choose the right film for your PV lamination process.

Read More
Robot String Cell Layup Machine  | Automated Solar Module Layup System - Ooitech
2025-09-05 22:01:28

Robot String Cell Layup Machine | Automated Solar Module Layup System - Ooitech

Ooitech HS-PBR Robot String Cell Layup Machine delivers high-precision automated string cell arrangement with ±0.3mm accuracy and ≤5s cycle time per string. Features CCD image system, robotic string handling, and compatibility with 60/72 cell, half-cell,

Read More
Gsolar Solar Panel Tester Sun Simulator GIV-20A2616 | A+A+A+ Class Solar Module IV Tester
2025-09-08 13:49:42

Gsolar Solar Panel Tester Sun Simulator GIV-20A2616 | A+A+A+ Class Solar Module IV Tester

Gsolar GIV-20A2616 A+A+A+ class solar panel tester and sun simulator with 2600mm x 1600mm testing area, 10ms-100ms long pulse duration, and GSN technology for accurate IV testing of crystalline, PERC, HJT, N-type, IBC, shingled, and half-cell solar module

Read More
Solar Panel Aluminum Frame – Anodized, G1/M6/M10/M12 Sizes
2025-09-10 10:28:35

Solar Panel Aluminum Frame – Anodized, G1/M6/M10/M12 Sizes

Solar panel aluminum frames – anodized, available for G1/M6/M10/M12 module sizes. Complete frame extrusion, cutting & assembly equipment by Ooitech for PV module production lines.

Read More
Portable HD EL Tester for Solar Module Inspection
2026-05-12 18:21:37

Portable HD EL Tester for Solar Module Inspection

Portable high definition EL tester with 24MP auto focus infrared camera for solar module electroluminescence testing, supporting USB and WiFi connection for laboratory and field inspection.

Read More