# Pinholes in TOPCon Cells: The Surprising Path

> New research reveals two types of SiOx pinholes in TOPCon cells. Passivating pinholes with residual oxygen actually boost efficiency to 26.55%

![Pinholes in TOPCon Cells: The Surprising Path](https://cdn.ooitech.com/static/upload/image/20260717/8f4e05ab43e74a832b2faee10f80bb99.webp)

- ** Jerry
- ** 2026-07-17
- ** 309 Views
- ** [Blog](./Blog.html)

Editorial responsibility for this article rests with **Wuhan Ooi Photoelectric Technology Co., Ltd.** Written and reviewed by the Ooitech editorial team. See our [editorial policy](/editorial-policy.html) for how we write, where AI tools are used, and how to request a correction.

## Pinholes in TOPCon Cells: The Surprising Path

**Quick answer:** Research on TOPCon cells has found that deliberately leaving a controlled amount of thin oxide can improve passivation rather than degrade it, which reverses a long-held assumption. The study measured oxide layers in the range of 0.2 nm and 0.3 nm against a reference at 1.7 nm, and found that the thinner, deliberately retained oxide did not simply add resistance. The tunnel oxide in a TOPCon cell has to be thin enough for carriers to tunnel through and thick enough to passivate the surface, and the conventional target sits at one or two nanometres. What the result suggests is that the boundary is less sharp than assumed, and that the chemical state of the interface matters as much as the thickness. For a production line, that shifts attention toward interface control rather than thickness alone.

PV Module Manufacturing · by Jerry, Ooitech

## Overview

Here is something that flips a long-held assumption in silicon PV. Researchers found that deliberately leaving certain "pinholes" in the SiOx layer of a [TOPCon](https://www.ooitech.com/what-is-topcon-solar-cell-a-complete-guide-to-tunnel-oxide-passivated-contact-technology.html) cell can push efficiency up to 26.55%, instead of dragging it down.

The key finding: pinholes in the tunnel oxide split into two families. One is the recombination type (oxygen-depleted, where poly-Si contacts c-Si directly, bad), the other is the passivating type (residual oxygen stays behind, passivating dangling bonds while still allowing tunneling, good). The passivating type measures about 1.6 ± 0.2 nm × 1.4 ± 0.3 nm in cross-section, with an areal density of 2 × 10¹² cm⁻². A Fischer model showed that what decides device performance is not pinhole geometry, but whether the pinhole is passivated.

Reference: *Passivating pinholes for large-area and high-efficiency silicon solar cells with tunnel oxide passivated contact*, Nat Commun 17, 2490 (2026). [https://doi.org/10.1038/s41467-026-70511-2](https://doi.org/10.1038/s41467-026-70511-2)

## Research Background and the Problem That Stuck

TOPCon is now the mainstream for n-type silicon. Runergy hit 26.55% on 335 cm², Jinko stacked TOPCon plus perovskite to 33.24%, and single-side n-TOPCon has a theoretical ceiling of 27.79%. But nobody had pinned down what role the pinholes in that interfacial SiOx layer actually play.

The traditional view: pinhole means poly-Si pokes straight into c-Si, oxygen passivation fails, bad news.

The reality is messier. Oxide too thick (>1.7 nm) passivates well but tunnels poorly, so FF collapses. Oxide too thin (<1.3 nm) means more pinholes, and now you worry about Voc collapsing.

The authors broke oxide thickness plus oxygen distribution into three cases (the Introduction section):

- Case 1: thick oxide, passivation OK, tunneling not optimal
- Case 2: thin oxide plus oxygen depletion, giving recombination-type pinholes (the classic "bad pinhole")
- Case 3: thin oxide but oxygen still seeps into the pinhole, giving passivating-type pinholes (the new finding here)

Before this, HR-TEM resolution wasn't good enough to see features below 2 nm. Literature reported pinhole diameters of 5 nm to 200 nm and densities of 10⁶ to 10⁸ cm⁻², which were all just "big holes". Selective etching and c-AFM rely on the etch rate difference between Si and SiOx, so regions with residual oxygen simply don't etch open. Passivating pinholes were naturally screened out by these methods. That's why Case 3 went unseen for so long.

## Mechanism: Two Types of Pinhole (Figure 2)

Aberration-corrected HAADF-STEM (JEM ARM200F plus Spectra 300, 200/300 kV) scanned the poly-Si/SiOx/c-Si interface on a high-efficiency wafer (25.40%) and a low-efficiency control (24.07%).

| Type | Oxygen state | Size (high/low efficiency) | EELS O-K edge |
| --- | --- | --- | --- |
| Recombination | Oxygen-depleted, poly/c-Si lattice directly joined | Low-efficiency wafer ~1.37 × 1.35 nm | Deep oxygen valley |
| Passivating | Residual oxygen present, dangling bonds passivated | High-efficiency wafer 1.55 × 1.25 nm | Oxygen signal still visible, shallow oxygen valley |

### Key point: the pinholes on the high-efficiency wafer are actually smaller, and retain oxygen better. All sizes are an order of magnitude smaller than earlier literature reported.

The Fischer point-contact model results (Fig. 3d in the original):

- Pinhole area fraction f = πr²/P², but J₀ is insensitive to f. What really dominates is the surface recombination velocity S at the pinhole.
- Around f ≈ 0.1, once S ≳ 10³ cm/s, J₀ climbs steeply, and it saturates above S > 10⁵ cm/s.
- Meaning: the key to high performance isn't "zero pinholes", it's "pinholes that are passivated". This is the biggest highlight of the whole paper.

On density, this is a bit of a revolution. Statistics from X-Y orthogonal slicing across 40 wafers (high plus low efficiency) gave 2 × 10¹² cm⁻² for passivating and 3 × 10¹² cm⁻² for recombination pinholes, 4 to 6 orders of magnitude higher than literature values.

Three reasons stack up: first, the concept changed, so previously screened-out passivating nanodefects became visible; second, the samples are industrially optimized wafers above 25%, not test structures; third, the method is atomic-level HAADF, and indirect approaches simply can't see the sub-2 nm oxygen-containing region. To guard against overlap along the beam direction from 50 to 150 nm thick TEM samples, the authors backstopped with 4D-STEM ptychography along the thickness direction, confirming the density statistics aren't distorted by projection overlap.

## Process Landing Point: Two-Step Oxidation plus Back Polishing plus Poly Triple Coupling

The variables from the original Methods plus SI (Supplementary Table 1):

- Two-step oxidation: first O₂ oxidation into thin SiO₂, then an oxygen-starved step (no oxygen fed in). The passivating type needs longer oxygen flow time, higher temperature, larger flow, and higher pressure, which favors uniform, dense oxide.
- POCl₃ diffusion: lower deposition temperature plus shorter time improves poly crystallization and suppresses recombination-type pinholes.
- Back polishing morphology sits upstream of oxide thickness uniformity. All three have to be tuned together to stably produce Case 3.

## Performance Comparison (Fig. 4 Hard Data)

Symmetric double-side poly-Si/SiOx samples (n-Si 1–3 Ω·cm, double-side polished):

- τeff: 8.9 ms high efficiency vs 2.96 ms control (injection 5×10¹⁵ cm⁻³)
- J₀: 2.6 vs 10.6 fA/cm²
- ΔVoc measured at 15.9 mV, but the J₀ difference alone explains only ~11 mV. The remaining ~5 mV the authors attribute to improved bulk SRH lifetime. The optimized anneal, while creating passivating pinholes, also getters metal impurities (citing Krügener's 25% POLO work). Fixing both interface and bulk together is the recipe for crossing 25%.

For FF, the difference mainly comes from Rs:

- Rs: 357 (high efficiency) vs 619 mΩ·cm² (control), Suns-Voc measured
- ρc (TLM): 4.6 vs 5.4 mΩ·cm²

The counterintuitive point: by "denser pinholes lower ρc" logic, more passivating pinholes on the high-efficiency wafer should mean lower ρc, and indeed 4.6 < 5.4. But the authors add a twist. Near recombination-type pinholes, phosphorus diffuses into the wafer, while passivating types are blocked by oxygen (the EDS doping profile in Supplementary Fig. 10). So doping profile and contact resistance follow two separate logics, and you can't explain them by pinhole density alone.

PL was uniform across the full wafer, and Corescan mapping of Voc distribution also held up for large-area uniformity.

## One Line for the Industry

This paper pushes the TOPCon interface from a binary story of "intact oxide vs pinhole leakage" to a ternary one: "pinholes can be good too, as long as oxygen is still there". What the industry needs to do next isn't to obsess over zero pinholes, but to tune the back polishing to oxidation to poly deposition chain so that pinholes carry oxygen. Daheng's wafer at 25.40% on 333.3 cm² has already proven the road works.

## Ooitech's View

What strikes us here is how much of this hinges on the process chain, not just the cell design. That two-step oxidation, POCl₃ tuning, and back polishing all have to move together is exactly the kind of coupling that gets lost when a line is assembled piecemeal. On the module side we see the same pattern, where lamination and stringing tolerances quietly decide whether a good cell keeps its Voc. If you want a closer look at how these interface-sensitive processes translate onto a real production floor, our factory walkthroughs on YouTube ([www.youtube.com/ooitech](http://www.youtube.com/ooitech)) are worth a subscribe.

## Further reading and background data

Public reference material on this topic, published by the organisations that maintain the industry's technology roadmap and market data:

- [VDMA — International Technology Roadmap for Photovoltaic (ITRPV)](https://www.vdma.org/international-technology-roadmap-photovoltaic)
- [Fraunhofer ISE — Photovoltaics Report](https://www.ise.fraunhofer.de/en/publications/studies/photovoltaics-report.html)
- [pv magazine — global PV industry news and technical coverage](https://www.pv-magazine.com/)

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Request A Quote

All uploads are secure and confidential.

## We deliver expertise you can trust our service

Direct-from-Factory Equipment.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

![](/template/ooitech/assets/img/icon/staff.svg)

### Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

![](/template/ooitech/assets/img/icon/certified.svg)

### 15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. [Know More **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

thank you for ooitech's professional support and on time after service.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra From Africa

![](/template/ooitech/assets/img/icon/quote.svg)

Thanks to Ooitech for providing highly suitable BC solar cell experimental equipment.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

![](/template/ooitech/assets/img/icon/quote.svg)

Thanks to Ooitech for providing the fully automated production equipment—your installation and after-sales service have been excellent.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

![](/template/ooitech/assets/img/icon/quote.svg)

Thank you again so much again for the very big big help for improving and fixing the factory and also teaching the workers how to use the machines

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

![](/template/ooitech/assets/img/icon/quote.svg)

A man with a big soul. Thank you very much for your visit Mr Wu. Thank you very much for the services provided in installing equipment and training my students. The kindest person and professional in his field

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

## Our Latest Products

![EVA Encapsulant Film: 80 N/cm Peel, EVA vs POE vs EPE](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774518543829873.webp)

- [** ooitech](./EVA-POE-EPE-Encapsulant-Film-for-Solar-Panel-Manufacturing-Complete-Technical-Guide.html)
- [** 89866](./EVA-POE-EPE-Encapsulant-Film-for-Solar-Panel-Manufacturing-Complete-Technical-Guide.html)

### EVA Encapsulant Film: 80 N/cm Peel, EVA vs POE vs EPE

EVA encapsulant film for solar modules, plus POE and EPE options: anti-PID, UV-resistant and compatible with TOPCon and PERC lines, in your thickness.

![STW-60A Shingled String Terminal Head: 20s/String](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774264892557837.webp)

- [** ooitech](./stw-60a-automatic-shingled-string-cell-terminal-head-welding-machine-solar-module-busbar-welding-equipment.html)
- [** 78315](./stw-60a-automatic-shingled-string-cell-terminal-head-welding-machine-solar-module-busbar-welding-equipment.html)

### STW-60A Shingled String Terminal Head: 20s/String

STW-60A automatic shingled string cell terminal head welding machine by Ooitech uses infrared heating technology to weld busbars on both positive and

![SC-10C Silicon Wafer Laser Cutting Machine](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774340166130021.webp)

- [** ooitech](./SC-10C-Full-Automatic-Silicon-Wafer-Laser-Cutting-Machine-High-Precision-Solar-Cell-Production-Equipment.html)
- [** 30196](./SC-10C-Full-Automatic-Silicon-Wafer-Laser-Cutting-Machine-High-Precision-Solar-Cell-Production-Equipment.html)

### SC-10C Silicon Wafer Laser Cutting Machine

SC-10C Full Automatic Silicon Wafer Laser Cutting Machine by Ooitech - High-speed precision cutting equipment for solar cell production with 860PCS/H

![DH200-Y Automatic Bussing Machine: 17s Cycle Time](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774348162498246.webp)

- [** Rachael](./automatic-bussing-machine-dh200-y-solar-panel-busbar-soldering-equipment-ooitech.html)
- [** 87987](./automatic-bussing-machine-dh200-y-solar-panel-busbar-soldering-equipment-ooitech.html)

### DH200-Y Automatic Bussing Machine: 17s Cycle Time

Ooitech DH200-Y Automatic Bussing Machine delivers high-speed electromagnetic busbar soldering with 17s cycle time

![GC-1500 EVA/TPT Online Cutting & Laying Machine](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774350387657887.webp)

- [** Rachael](./gc-1500-eva-tpt-online-cutting-and-laying-machine-automatic-solar-panel-eva-backsheet-cutter-ooitech.html)
- [** 37593](./gc-1500-eva-tpt-online-cutting-and-laying-machine-automatic-solar-panel-eva-backsheet-cutter-ooitech.html)

### GC-1500 EVA/TPT Online Cutting & Laying Machine

GC-1500 EVA/TPT Online Cutting & Laying Machine by Ooitech features automatic EVA, POE, and backsheet cutting and laying for solar panel production

![PV Ribbon Machine: Wire Drawing for Solar Ribbon](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026051187922761.webp)

- [** ooitech](./wire-drawing-machine-for-solar-ribbon-production-line.html)
- [** 736](./wire-drawing-machine-for-solar-ribbon-production-line.html)

### PV Ribbon Machine: Wire Drawing for Solar Ribbon

Professional intermediate wire drawing machine for solar ribbon production line, featuring four-axis horizontal design