# LONGi ACM: What Silver-Free Metallization Does to a Joint

> LONGi's ACM swaps silver paste for a printed copper-alloy electrode. What the three-layer stack does to the joint, and which stringer fits each cell case.

![LONGi ACM: What Silver-Free Metallization Does to a Joint](https://cdn.ooitech.com/static/upload/image/20261030/acm-two-part-electrode-printed-alloy.png)

- ** Ooitech Editorial Team
- ** 2026-11-23
- ** 0 Views
- ** [Photovoltaics & Applications](./Photovoltaics.html)

Editorial responsibility for this article rests with **Wuhan Ooi Photoelectric Technology Co., Ltd.** Written and reviewed by the Ooitech editorial team. See our [editorial policy](/editorial-policy.html) for how we write, where AI tools are used, and how to request a correction.

## LONGi ACM: What Silver-Free Metallization Does to a Joint

**Quick answer:** ACM is LONGi's silver-free metallization for back-contact cells, announced in July 2026 and in volume production at its Xixian base. It stacks three things: a seed and barrier layer that keeps copper out of the silicon, a copper-alloy conductor printed with existing screen tools, and a matrix contact geometry in which every electrode has a wide transport part and a small contact point. The published figures are 27.6% cell efficiency certified at ISFH, 672 W certified at TUV Rheinland, 0.2 to 0.3 points of cell gain, 3 to 5 W of module gain, and about 80% less risk of a broken finger. What reaches the stringer is a shorter list than that: a flat bar to join to, a metallization that has already spent its last high-temperature step, a contact path that runs through discrete points, and no field data yet.

The interesting part of ACM is not the missing silver. It is that the electrode was redesigned into two parts, and only one of them is the surface your ribbon lands on.

## What LONGi launched, and when

LONGi announced ACM in July 2026 as nano-alloy matrix contact and said it had reached volume production at Xixian. The company presents it as the core silver-free metallization for its own back-contact line, compatible with HPBC, HIBC and BC 2.0. In LONGi's framing it is one block of a larger set: a conductive backsheet handles architecture, shingling and hidden busbars handle layout, ACM handles the metal.

One caveat belongs near the top. LONGi has not published the alloy composition or the residual silver content, and [an earlier review of the silver-free routes on this site](https://www.ooitech.com/the-silver-free-debate-returns-less-silver-copper-paste-or-copper-plating-which-route-is-more-reliable.html) already placed ACM in the copper-based paste family rather than in a pure copper category. Read the phrase about replacing silver paste as a description of a material, not an assay.

## The silver arithmetic, and why one metal is not enough

Proven silver reserves are about 640,000 tons, annual mine output about 32,000 tons, and photovoltaic manufacturing already takes more than a quarter of global consumption. The source adds a widely repeated projection: at 1,000 GW a year of module output, the industry runs out of affordable silver inside a decade.

That number is quoted far more often than it is checked. A quarter of 32,000 tons is 8,000 tons a year, and 640,000 divided by 8,000 gives 80 years, not 10. The ten-year version holds only if PV demand grows several times from here, so it is a growth scenario, not a reserve calculation. The figure that matters commercially is smaller: 8,000 tons over 1,000 GW is 8 mg per watt, so a 672 W module carries about 5.4 g of silver.

The old answer to silver cost was geometry. Front fingers went from about 110 micrometers to under 20 today, and every micrometer removed took conducting cross-section with it. Thinner fingers raise resistance, and eventually they break, lift or fail to wet. That is the triangle the source describes, with silver in the middle.

Copper conducts about as well as silver and costs far less, so why not simply swap the paste? Two properties answer it. Copper oxide is closer to an insulator than to a conductor, so an oxidized finger stops working instead of aging gently. And copper diffuses through silicon far faster than silver, creating deep levels that cut lifetime and, at a contact, a path where current should not flow. Li Zhenguo closes it in one line: in the end, we did not choose a single metal.

## Three layers, one job each

The first is a seed and barrier film a few nanometers thick between silicon and the conductor. It does two things: make a low-resistance ohmic contact to the doped silicon, and stop copper crossing into it. The source says the industry speculates about nickel, which would form a nickel silicide, or a titanium tungsten barrier. LONGi has confirmed neither.

The second is the conductor, described as a multi-metal alloy paste rather than a single element, wrapped in a polymer shell that keeps oxygen off the metal under it. The claim attached to it is compatibility with screen printing, which is why the retrofit story is short: the same printer, a different paste.

The third is not a layer at all but a geometry, and it is the part that changes what a stringer sees.

| Layer | What it is | What it decides at the joint |
| --- | --- | --- |
| Seed and barrier | A nanometer-scale film between silicon and the conductor; the source says the industry speculates about nickel or a titanium tungsten barrier | Contact resistance, and how much heat the interface takes before the barrier stops being one |
| Copper-alloy conductor | A multi-metal alloy paste printed with screen tools, wrapped in a polymer shell that keeps oxygen off the metal | The metal thickness the ribbon sits on, and the surface temperature it tolerates without losing its shell |
| Matrix contact | A point array where current enters the silicon, with a wider transport part above carrying it out | How much area the ribbon bonds to, and how pull strength and thermal cycling are measured |

### The wet route it replaces

Plating is the reference process the industry has run for years. Its steps:

- Deposit a barrier layer and a seed layer on the cell surface.
- Coat the whole surface with a mask, then expose and develop the pattern.
- Etch the seed and barrier wherever the mask was removed.
- Strip the remaining mask with a laser, then clean the oxide off the seed with acid.
- Plate copper into the openings to build the electrode.

Each of those steps is wet or lithographic and registered to the last. ACM's claim is that a printed alloy replaces the sequence, which is why LONGi calls the retrofit simple: no plating bench, no mask, no strip. The source calls the result a dry, simplified version of plating.

The number to hold onto is the aspect ratio. Five to seven times the cross-section at a narrower width is not a small rheology problem, and if it holds in volume it is worth checking on incoming cells rather than on a slide. A polished cut and a four-point probe need no disclosure from the supplier.

## The electrode has two parts, and only one of them is a joint

One electrode, two jobs. The ribbon bonds to the transport bar; the contact point underneath sets recombination, and the joining heat runs straight down to it. Structure as described in LONGi launch material, redrawn in English.

Inside one electrode there are two shapes. A contact part passes through an opening in the passivation and touches the doped layer over a small area. A transport part is a wide flat bar above it, carrying current sideways to the ribbon. The figure shows both views.

The reason is arithmetic. Recombination loss scales with contact area and resistive loss scales with cross-section, so the design separates them. Li's comparison in the source is a high-speed train that only stops at stations: current enters at few places and then travels a long way without paying for it.

For a module line one consequence is easy to miss. The ribbon does not bond to a point contact but to the transport bar, which is flat, wide and printed rather than fired, while everything thermal underneath is a point. **The joint never touches the silicon. It touches the bar that feeds the points, and its heat runs straight down to the thinnest part of the barrier.**

So pull strength belongs per pad, because the bond area is the bar and the bar is not the cell. Placement tolerance belongs at the pad edge. The thermal budget belongs to the cell stack, which no longer has a firing step to absorb an overshoot.

## What LONGi published

The figures below are as published by LONGi and reported in the source, with the certification body named where one is named. None were measured by us.

| Metric | Figure | Status |
| --- | --- | --- |
| Cell efficiency, volume data | +0.2 to 0.3 points | LONGi, as reported |
| Module power, volume data | +3 to 5 W | LONGi, as reported |
| Cell efficiency, certified | 27.6% | ISFH, per the source |
| Module power, certified | 672 W | TUV Rheinland, per the source |
| Finger cross-section | 5 to 7 times a conventional finger | LONGi, as reported |
| Finger resistance | 1/5 to 1/7 of a silver finger | LONGi, as reported |
| Broken-finger risk | about 80% lower | LONGi, as reported |
| Warranty | 1% year one, 0.33% a year, 30 years | LONGi warranty terms |

Two conversions are ours. A gain of 0.2 to 0.3 points on a cell above 27% is about 1% relative, and 3 to 5 W on a 640 to 672 W module is 0.5% to 0.8%. Five to seven times the cross-section at a narrower width means five to seven times the height, which is the aspect ratio printing has to hold in production.

## The reliability file, and the line it has not crossed

### What the tests show

The laboratory work goes past the standard sequence: 2,000 hours of damp heat, three times the thermal cycling sequence, and twice the UV60 dose. One cycling run produced an unplanned result worth more than a planned one: the chamber outlet rose to 150 Celsius, and the ACM modules survived it while conventional modules showed microcracks and darkening. Silver paste is fired hot and keeps porosity that takes up moisture over years; the ACM conductor is a low-temperature film and starts without it. The warranty terms follow: 1% in year one, 0.33% a year after that, 30 years.

In our environmental testing runs, we subject laminated modules to 2,000 hours of damp heat to verify that encapsulation maintains bond integrity around the polymer-protected alloy without edge delamination or moisture ingress.

### What they cannot show

What the file cannot cover is time. Volume production began in mid-2026, so there are months of outdoor exposure and nothing close to a 25-year claim. The failure mode is slow: copper diffuses through silicon more than a thousand times faster than silver, and once it reaches the emitter it forms recombination centers that do not anneal out. The industry has run this experiment: early copper plating passed laboratory testing, then lost output after about two years in the field. LONGi's three-layer design is aimed at exactly that history, but no company can show 25 years of it. Potential-induced degradation is the cautionary case: it passed accelerated tests, shipped, and surfaced later in the field.

The source puts a date on the gap. Silver-reduced modules made before 2026 need until about 2031 to accumulate five years of outdoor data, and that is when the question stops being a debate and becomes a measurement.

## What this changes at the stringer

The surface is printed, not fired. A silver pad is a sintered, fairly inert film; an alloy bar under a polymer shell is neither, and that shell is what stands in for silver's stability. Any joining step that burns, abrades or chemically strips it works against the design.

The heat budget now belongs to the cell. ACM removes the high-temperature sintering step, so the metallization arrives with no thermal margin left. Where the ceiling sits depends on the passivation stack, and with an amorphous silicon layer it sits well below a conventional firing profile. [The structure of a back-contact cell](https://www.ooitech.com/bc-solar-cells-explained-structure-differences-manufacturing-process-and-string-soldering-principle.html) sets that geometry; the ceiling is set by whatever sits on top of it.

To respect the lower heat ceiling of these cell stacks, we operate lamination cycles below 150 Celsius, using precise platen heating zones to avoid localized thermal overshoot on the printed contacts.

The area is a bar and the path is a point. Bond area follows the transport bar, so a flat ribbon still has real area to land on, while the thermal path below runs through discrete points, where a pull test and a thermal cycle both concentrate.

### Which machine for which cell

If the cell is rear-only back contact with a low-temperature stack, the joint is dispense, place and cure, and the class is the one built for BC rear joining: [OSLB-1300](https://www.ooitech.com/oslb-1300-back-contact-cell-welding-machine-bc-solar-cell-stringer-for-ibc-abc-hpbc-panel-production.html), quoted at 1,000 cells per hour or better, 0.10 mm placement, four glue sets, CCD corner detection.

If the cell maker qualifies a short IR window at the pad, the flat-ribbon class applies: [SS-1500B](https://www.ooitech.com/SS-1500B-Automatic-Solar-Cell-Welding-Machine-High-Speed-Tabber-Stringer-for-BC-TOPCON-PERC-Cells.html), which takes ribbon 0.35 to 1.0 mm wide and 0.12 to 0.25 mm thick at 0.15 mm placement. The difference between the two is not throughput. It is whether the cell tolerates a local peak.

The front-side MBB class, such as [AM050FH](https://www.ooitech.com/am050fh-mbb-pv-cell-soldering-stringer-fully-automatic-solar-cell-tabber-stringer-machine-ooitech.html), does not apply here: ACM as launched is a rear-only geometry. If it later moves to a cell with front-side contacts, that class becomes relevant again, and not before.

| Cell case | What the joint is | Machine class | What the specification fixes |
| --- | --- | --- | --- |
| Rear-only back contact, low-temperature stack | Dispense glue, place ribbon, cure | OSLB-1300 | Glue pattern per pad, cure peak and dwell, 0.10 mm placement |
| Rear contact with a qualified IR window | Flat ribbon soldered to the transport bar | SS-1500B | Ribbon 0.35 to 1.0 mm wide, 0.12 to 0.25 mm thick, peak at the pad, 0.15 mm placement |
| Front-side MBB TOPCon or PERC, not this case | Round wire soldered to front busbars | AM050FH | 0.20 to 0.26 mm wire, 3BB to 24BB, 0.05 mm placement |

## How to write it into a purchase order

Five items belong in the specification rather than in a conversation, because none appear on a module datasheet and all of them move takt time.

- The pad drawing, with transport bar width and contact pitch, so the vision recipe and nozzle pattern come from geometry rather than a photograph.
- Pull strength per pad after damp heat, not before.
- The maximum temperature the metallization tolerates and the time allowed at it.
- Whether the polymer shell survives your flux chemistry, or the process has to be flux-free.
- Incoming EL or PL criteria, because broken-finger risk is a cell property.

That list is the one a BC line already keeps for its own pad geometry, plus one addition: the metal now has a thermal history instead of a refractory film. [Insulating glue on the rear](https://www.ooitech.com/why-do-bc-solar-cells-need-insulating-glue-on-the-back.html) was the first such interface; the joint is the second.

## What would change our mind

- Three years of field data from a hot, humid site, with modules opened and the emitter profiled for copper.
- A disclosure of residual silver, so the label can be checked against a number.
- Module-level damp heat and thermal cycling on ACM-jointed strings, not only on cells.
- Pull strength after 1,000 hours of damp heat, on the ribbon a customer would actually run.

If those land, the joint stops being the risk.

## Where these numbers come from

The structure, layer functions, quoted remarks, certification values and warranty terms come from a Chinese technical explainer on the ACM platform published in October 2026, drawing on launch material and Li Zhenguo's public remarks. The reserve and production figures, the finger-width history and the ten-year scenario are that source's. The division, the per-watt conversions, the aspect-ratio reading and the machine mapping are ours.

Nickel silicide and titanium tungsten appear in the source as speculation about undisclosed materials, and they appear that way here. We have not tested, disassembled or sold any cell discussed, and no figure in the tables was measured by us.

## FAQ

### Q: Is ACM really silver-free?

LONGi describes it as a full replacement of silver paste, but the composition is undisclosed, and a copper-based paste can still carry a little silver in a seed or contact layer. Ask for the assay, not the adjective.

### Q: Does an ACM cell need a different stringer?

Not a different platform, a different budget. The pad is a printed alloy bar, the stack sets the ceiling, and the joint is glue and cure or a short pulse. What changes is the window, not the class.

### Q: Can an ACM cell be soldered with an IR lamp?

Only if the cell maker qualifies a window at the pad. ACM removes the sintering step, so the metallization has no margin left to absorb an overshoot. A supplier who has qualified one will state the peak and the dwell.

### Q: What temperature must the joint stay under?

There is no single number, and anyone quoting one is guessing. The ceiling comes from the cell stack, and on a cell with an amorphous silicon layer it is set by that layer, well below a firing profile.

### Q: Does the finer finger change the ribbon width?

Not directly. The ribbon bonds to the transport part, so width follows the pad layout rather than the finger. What changes is the pull specification and the placement tolerance.

### Q: Why does one electrode have two parts?

Because recombination scales with contact area and resistance scales with cross-section. A wide bar over a small point gets low resistance with little contact area, which is the whole reason for the geometry.

### Q: Is ACM only for back-contact cells?

As launched, yes, aimed at HPBC, HIBC and BC 2.0. A front-side cell has a different shading and adhesion problem, and nothing in the launch material addresses it.

### Q: When will there be field data?

Production started in mid-2026, so one to three years of plant data means 2027 to 2029, and the industry estimate for five-year data is around 2031. Until then the evidence is accelerated aging.

## Final thoughts

ACM matters to a module line for a narrow reason. It takes the last high-temperature step out of the metallization and puts the whole thermal budget into the joint, just as the metal becomes a printed alloy under a polymer shell. Whether the copper stays put for 25 years has no public answer. Buy the machine that can hold a narrow window for a decade.

For back-contact modules with reduced thermal margins, OOITech supplies single and double chamber [solar panel laminator machines](https://www.ooitech.com/solar-panel-laminator-machine.html) in oil-heated and electric configurations. Our equipment provides uniform temperature control across the platen to protect sensitive rear metallization. Send your drawings, module stack, or test samples to our team for process evaluation.

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Request A Quote

All uploads are secure and confidential.

## We deliver expertise you can trust our service

Direct-from-Factory Equipment.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

![](/template/ooitech/assets/img/icon/staff.svg)

### Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

![](/template/ooitech/assets/img/icon/certified.svg)

### 15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. [Know More **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

Thank you again so much again for the very big big help for improving and fixing the factory and also teaching the workers how to use the machines

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

![](/template/ooitech/assets/img/icon/quote.svg)

A man with a big soul. Thank you very much for your visit Mr Wu. Thank you very much for the services provided in installing equipment and training my students. The kindest person and professional in his field

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

![](/template/ooitech/assets/img/icon/quote.svg)

thank you for ooitech's professional support and on time after service.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra From Africa

![](/template/ooitech/assets/img/icon/quote.svg)

Thanks to Ooitech for providing the fully automated production equipment—your installation and after-sales service have been excellent.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

![](/template/ooitech/assets/img/icon/quote.svg)

Thanks to Ooitech for providing highly suitable BC solar cell experimental equipment.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

## Our Latest Products

![BC Cell Tabber Stringer: 1000 Cells/h for IBC, ABC, HPBC](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032311945973.png)

- [** ooitech](./oslb-1300-back-contact-cell-welding-machine-bc-solar-cell-stringer-for-ibc-abc-hpbc-panel-production.html)
- [** 99199](./oslb-1300-back-contact-cell-welding-machine-bc-solar-cell-stringer-for-ibc-abc-hpbc-panel-production.html)

### BC Cell Tabber Stringer: 1000 Cells/h for IBC, ABC, HPBC

A BC cell tabber stringer welds IBC, ABC and HPBC cells on the rear face: 0.2 mm placement, 1000 cells/h, 0.2% breakage on Class A wafers.

![C350-CQC EVA & TPT Strip Cutting Machine: 30-80mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032714363679.webp)

- [** Rachael](./ECPC-C350-CQC-Punching-and-Cutting-Machine-High-Precision-Solar-Panel-Material-Processing-Equipment.html)
- [** 34861](./ECPC-C350-CQC-Punching-and-Cutting-Machine-High-Precision-Solar-Panel-Material-Processing-Equipment.html)

### C350-CQC EVA & TPT Strip Cutting Machine: 30-80mm

C350-CQC punching & cutting machine – 30 pcs/min, ±0.2mm accuracy for EVA, TPT & PPE solar materials. Precision processing for busbar and

![STW-60A Shingled String Terminal Head: 20s/String](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774264892557837.webp)

- [** ooitech](./stw-60a-automatic-shingled-string-cell-terminal-head-welding-machine-solar-module-busbar-welding-equipment.html)
- [** 78388](./stw-60a-automatic-shingled-string-cell-terminal-head-welding-machine-solar-module-busbar-welding-equipment.html)

### STW-60A Shingled String Terminal Head: 20s/String

STW-60A automatic shingled string cell terminal head welding machine by Ooitech uses infrared heating technology to weld busbars on both positive and

![PV Ribbon Production Line: Drawing, Rolling, Tinning](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026051194879300.webp)

- [** ooitech](./pv-busbar-ribbon-integrated-drawing-rolling-tinning-production-line.html)
- [** 834](./pv-busbar-ribbon-integrated-drawing-rolling-tinning-production-line.html)

### PV Ribbon Production Line: Drawing, Rolling, Tinning

Professional integrated PV busbar ribbon production line combining wire drawing, rolling, flat drawing, annealing and tin coating processes for high

![SC-10C Silicon Wafer Laser Cutting Machine](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774340166130021.webp)

- [** ooitech](./SC-10C-Full-Automatic-Silicon-Wafer-Laser-Cutting-Machine-High-Precision-Solar-Cell-Production-Equipment.html)
- [** 30285](./SC-10C-Full-Automatic-Silicon-Wafer-Laser-Cutting-Machine-High-Precision-Solar-Cell-Production-Equipment.html)

### SC-10C Silicon Wafer Laser Cutting Machine

SC-10C Full Automatic Silicon Wafer Laser Cutting Machine by Ooitech - High-speed precision cutting equipment for solar cell production with 860PCS/H

![Solar Panel Production Line: Configurations from 5 MW to 1 GW](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032510951634.webp)

- [** ooitech](./solar-panel-production-line.html)
- [** 135](./solar-panel-production-line.html)

### Solar Panel Production Line: Configurations from 5 MW to 1 GW

Solar panel production line guide: stations, semi-automatic vs automatic, 5 MW to 1 GW configurations, layout, utilities, staffing and RFQ tips.