# Laser-Cut Edges in TOPCon: Passivating the Cross-Section

> A laser cut leaves bare silicon on both walls of a four-cut cell. Coating that wall with a tunnel oxide and doped poly-Si turns it into a contact.

![Laser-Cut Edges in TOPCon: Passivating the Cross-Section](https://cdn.ooitech.com/static/upload/image/20261016/2026101624242424.webp)

- ** Ooitech Editorial Team
- ** 2026-10-24
- ** 197 Views
- ** [Photovoltaics & Applications](./Photovoltaics.html)

Editorial responsibility for this article rests with **Wuhan Ooi Photoelectric Technology Co., Ltd.** Written and reviewed by the Ooitech editorial team. See our [editorial policy](/editorial-policy.html) for how we write, where AI tools are used, and how to request a correction.

## Laser-Cut Edges in TOPCon: Passivating the Cross-Section

**Quick answer:** Cutting a cell into quarters splits it along a laser groove, and that groove leaves bare silicon on both walls. The published approach is to grow a thin tunnel oxide on the wall, deposit n⁺ doped poly-Si over it and cap the poly-Si with AlOₓ, so the cut face behaves like a selective contact instead of a recombination centre. Every added step is low temperature, which is what makes it interesting to a line that already runs LPCVD.

Four-cut and multi-cut cells are now ordinary production, and the reason is arithmetic: splitting a cell into four lowers the current each ribbon carries, shortens the path across the fingers and cuts resistive loss in the interconnection. The gain is real and it is why [four-cut TOPCon cells](https://www.ooitech.com/topcon-four-cut-cells-how-cutting-a-cell-into-four-increases-power-output.html) became the default before anyone argued about the cost.

The cost sits on the cut itself. A laser groove separates the quarters, and the wall it opens is silicon that has never had a passivation layer on it. Surface states there sit in the middle of the band gap, and carriers that reach the wall recombine. That is a voltage loss, not a shading loss, and it does not show up in any measurement taken before the cutting step.

The approach described below stops treating that wall as damage to be minimised and treats it as a surface to be coated. It is the same selective-contact idea TOPCon already uses on the wafer face, applied to a surface that cutting created a few process steps earlier.

## The cut edge is a surface, and it is the worst one on the cell

Every other silicon surface in a finished module has been through the full passivation sequence: texturing, cleaning, a dielectric stack, sometimes a doped layer underneath it. The groove wall gets none of that. It is created after the front junction is formed and after the rear stack is deposited, so what the laser leaves behind is the raw material.

The numbers usually quoted for that kind of surface are discouraging. Interface state densities around 1 × 1012 cm−2 eV−1 and a surface recombination velocity above 500 cm/s, both reported for the as-cut case in the source this article draws on. Against a passivated surface measured in single-digit cm/s, an untreated cut edge recombines roughly two orders of magnitude faster.

What makes it matter is not the area. A cross groove is 30 µm wide and about 1.5 µm deep, and cutting an M10 cell into four opens roughly a square millimetre of wall against the 33,000 mm2 of wafer face. Rather, it is that carriers generated within a diffusion length of the cut can reach it, and the wall runs the full length of the cell in both directions. Line length is what the loss scales with, and the cross pattern puts a long line through the middle of every quarter.

This is also why the loss behaves like a voltage problem. Recombination at the edge removes carriers from the bulk, and open-circuit voltage responds to the total recombination rate across the cell. The filler factor moves too. Shading would show up in current; this shows up in Voc and FF, which is a less obvious place to look when a cutting process is being qualified.

## What the coating actually is

The published structure puts three layers on the cut wall, in a specific order. Reading outward from the silicon: a very thin silicon oxide that carriers can tunnel through, a heavily doped polysilicon layer that carries them away, and an aluminium oxide cap that finishes the chemical passivation of the interface.

| Layer on the cut wall | Thickness | What it does |
| --- | --- | --- |
| Tunnel oxide, SiO2 | about 1–1.2 nm | Thin enough for carriers to tunnel through, thick enough to keep the metal and the doped layer off the silicon surface |
| Doped poly-Si | 80–120 nm | Carries the collected carriers sideways and sets the work function that makes the contact selective |
| AlOx cap | about 10 nm | Chemical passivation of the remaining interface states, plus a barrier against contamination |

Two details separate this from simply re-growing an oxide. First, the stack is not a dielectric only; it contains a doped semiconductor, so it can also conduct. A pure oxide would passivate the wall and leave it electrically dead, which is fine for a surface that collects nothing, but the wall here sits between two quarter cells that both need to move current. Second, the thicknesses matter in a way they do not on a flat wafer. The poly-Si has to be thick enough to stay continuous over a 1.5 µm deep groove with a rounded bottom. It also has to be thin enough that its own stress does not crack or peel it off the wall.

The source gives 120 nm for the poly-Si in the structure description and 80 nm in the process sequence, and remarks that 80 nm is enough for the field passivation effect. That difference is worth noting rather than smoothing over: it suggests the layer thickness is a tunable within the process window, not a fixed target, and that both values are within the range the authors consider workable.

## Why a thin oxide and a doped layer filter carriers

The mechanism is band engineering rather than chemistry, and it is the same one that made TOPCon competitive in the first place. On the bare wall, interface states are distributed across the band gap. An electron that reaches one of those states has somewhere to sit, and a hole arriving at the same state closes the circuit: the two recombine, and the pair is lost.

Once the oxide and the doped poly-Si are in place, the band structure at the interface is no longer flat. The thin oxide blocks the direct path between silicon and the doped layer while remaining thin enough for electrons to tunnel through it. The charge in the doped layer bends the bands in the silicon just below the interface, which is what creates the asymmetry: one carrier type sees a low barrier and passes, the other sees a high barrier and turns back.

The reported result is a fall in surface recombination velocity at the cut edge from about 500 cm/s to under 10 cm/s, a change of roughly 98%. That is a large number, and it is large for a simple reason: the starting point is an unpassivated surface, which is close to the worst case available. Improving a passivated surface by the same factor would not be possible.

It is worth being precise about what the coating does not do. It does not remove the groove, does not restore the silicon that the laser ablated, and does not make the wall optically useful. The quarter is still narrower. The claim is narrower than that: the cut face stops acting as a place where carriers die, and starts acting as a place where they can be collected.

## Where the process steps land

The route published with this structure is a normal TOPCon sequence with one insertion: after the laser has cut the cross groove, the wall is oxidised and re-doped before the cell-level passivation stack is deposited. Everything else stays where it was.

| Step | Published condition | Why it is set that way |
| --- | --- | --- |
| Laser cross grooving | 30 µm wide, 1.5 µm deep | Deep enough to separate the quarters cleanly, shallow enough to limit the wall area and the mechanical damage around it |
| Ozone oxidation | 90 °C, 30 s, about 1 nm | Grows a uniform oxide without the thermal budget that would disturb the junction already in the wafer |
| LPCVD poly-Si | 80 nm, doped in situ | Doping during deposition avoids a separate diffusion step and gives a controllable concentration gradient through the layer |
| Activation anneal | 750 °C, 20 min | Activates the dopant and crystallises the layer, which is what turns it into a conductor rather than a dielectric |
| Groove rounding | 2 s TMAH after grooving | Blunts the sharp groove corners where cracks and coating discontinuities start |
| Crystallinity check | Raman, above 80% | An incompletely crystallised layer passivates poorly and conducts worse, so it is treated as a measurable output |

The TMAH rounding and the crystallinity check are the two details that make this look like a production route rather than a laboratory demonstration. A 1.5 µm groove has a corner, and corners are where deposited films go thin and where stress concentrates. Rounding the corner for two seconds costs almost nothing and removes a class of failure that would otherwise appear later, in thermal cycling or in handling.

For a line, the interesting part is that none of the added steps needs a new tool. Oxidation, deposition and anneal all fit inside the LPCVD capacity a TOPCon line already has, and the two added steps are low temperature, so the thermal budget of the finished cell is not disturbed. The source reports line tact loss under 3%, which is the number to check first when a new step is proposed: a step that improves efficiency by half a point but costs 10% of throughput is a different proposal from one that costs 3%.

The back end of the sequence changes too, and not because of the coating. A four-cut cell that keeps its 12BB layout has to be strung from quarter cells, and the cut edge is now a surface the stringer handles. Placement tolerance, the force the ribbon applies at the joint and the amount of heat the cell sees during soldering all act on a piece whose edge has a 30 µm groove through it. That is where [fine-wire tabbing and stringing](https://www.ooitech.com/am050fh-mbb-pv-cell-soldering-stringer-fully-automatic-solar-cell-tabber-stringer-machine-ooitech.html) equipment and the [bussing step](https://www.ooitech.com/automatic-bussing-machine-dh200-y-solar-panel-busbar-soldering-equipment-ooitech.html) meet the cell design, and it is the part of the flow the coating does not address.

## What the reported comparison shows

The source prints a before-and-after comparison for a standard four-cut cell and the same cell with the coated edge. The table below reproduces it. These are the numbers published with the route; they come from one source, and we have not verified them independently.

| Parameter | Standard four-cut | With passivated edge | Change |
| --- | --- | --- | --- |
| Edge SRV (cm/s) | 500 | under 10 | −98% |
| Open-circuit voltage (mV) | 736 | 744 | +8 mV |
| Short-circuit current (mA/cm2) | 40.8 | 41.0 | +0.2 |
| Fill factor (%) | 84.0 | 84.5 | +0.5 |
| Cell efficiency (%) | 25.3 | 25.8 | +0.5 absolute |
| Bifaciality (%) | 85 | 90 | +5 points |

Read the pattern rather than the individual values. The voltage gain is larger than the current gain, which is what the mechanism predicts: recombination at a surface costs voltage first. The fill factor moves slightly, consistent with a small reduction in the fraction of the area that is electronically dead. Efficiency follows the voltage, and 0.5 points absolute is the headline claim.

The bifaciality figure deserves more caution than the rest. Going from 85% to 90% is a five-point jump caused by a change on a surface that is a small fraction of the cell's rear area, and the source does not explain the mechanism. It could be real if the cut edge was previously a local shunt path on the rear, but it is also the kind of number that a single small sample can produce. Treat it as the least supported line in the table.

## What is not settled yet

Four things are missing from the published case, and all four matter before a line commits.

- **Reliability data on the coated edge.** A 1 nm oxide and a 10 nm aluminium oxide cap on a groove wall see the same damp heat, thermal cycling and mechanical load as the rest of the cell. A cut edge is also a stress raiser under thermal cycling, because two quarter cells expand against a groove. None of that appears in the comparison table.
- **The thickness question.** The source gives two different poly-Si thicknesses for the same structure. That is not a contradiction, but it does mean the optimum is not pinned down, and thickness affects stress, deposition time and tact together.
- **Independent replication.** The efficiency gain comes from one reported data set. A 0.5 point absolute gain is large enough to be worth chasing and large enough to be worth double-checking on a different line and a different paste and ribbon combination.
- **The interaction with the rest of the cell.** Adding a doped layer on the groove wall changes what that wall does electrically between two quarters. How it interacts with the rear metallisation pattern and with the stringing of quarter cells is a system question, not a coating question.

There is a broader point in the same direction. Cutting a cell is a trade that was accepted on the strength of the interconnection gain alone. The [four-cut framework](https://www.ooitech.com/four-cut-cell-technology-the-next-efficiency-code-in-the-pv-industry.html) treats the cut as a given, and the [multi-cut analysis](https://www.ooitech.com/multi-cut-solar-modules-a-practical-analysis-of-shade-resistance.html) looks at what the smaller cell does to shading and to module layout. Work on the cut edge attacks the cost side of that trade, and if it holds up it changes the optimum number of cuts rather than just improving the existing one.

## How to read this against the rest of the cutting conversation

Three separate ideas are usually mixed together when four-cut cells come up, and keeping them apart makes the literature easier to read.

The first is the interconnection gain: quarter cells carry a quarter of the current, so resistive loss in the ribbon falls sharply. That is settled and it is why the technology is in production. The second is the module-level consequence, where smaller cells change shade tolerance, junction box requirements and the mechanical behaviour of the laminate; the [two-part junction box](https://www.ooitech.com/why-topcon-four-cut-modules-need-two-part-junction-boxes-a-look-at-pv-junction-box-evolution.html) is one visible outcome. The third is the cut surface itself, which is the subject here and which the first two conversations tend to skip.

The practical link between them is the process flow. Grooving is done by a [laser cutting step](https://www.ooitech.com/SC-20P-Automatic-Solar-Cell-Laser-Cutting-Machine-High-Precision-BC-Cell-Processing-Equipment.html), the coating step lands in LPCVD capacity the line already owns, and the finishing steps are [metallisation](https://www.ooitech.com/pv-cell-metallization-can-the-silver-blocking-playbook-be-used-to-stop-copper.html) and stringing. A line evaluating this route is really evaluating whether the insertion fits between two tools it already has, and the published tact number is about 3%.

## FAQ

### Does the coating remove the need for cutting?

No. The quarters are still cut and the groove is still there. What changes is the electrical behaviour of the wall the groove exposed, not the geometry.

### Why not simply cut with a gentler process?

A cleaner cut reduces the damage but still leaves an unpassivated surface. The recombination comes from the missing passivation as much as from the roughness, which is why the answer here is a coating rather than a better laser recipe.

### Is a 1 nm oxide reliable?

Tunnel oxides of that order are already used in TOPCon production, so the concept is proven on the wafer face. Whether the same thickness survives on a groove wall, which has a different surface orientation and a rougher starting point, is one of the open questions.

### Does this apply only to TOPCon?

The tunnel-oxide and doped-poly-Si combination is a TOPCon structure, so the route is naturally aimed at lines that already run it. Other cell types cut into pieces would need a passivation stack compatible with their own process, which is a different engineering problem.

### What would we check first on a trial?

The edge SRV proxy and the voltage, before anything else. Deposition uniformity along a 30 µm wide groove, the crystallinity of the layer, and the tact cost of the inserted steps come next, and the mechanical behaviour of the quarter after grooving is the item most likely to be forgotten.

### Does the coating change what the stringer has to do?

Not directly. The coating is electrical, so placement accuracy, soldering temperature and handling force are unchanged. The quarter cell itself, with a groove through it, remains the harder object to handle, and that is a separate constraint from the one this work addresses.

## Final thoughts

Cutting silicon to make cells better is a slightly strange trade, and it works because the interconnection gain is large. What this piece of work does is close the loop on the part of the trade that was never priced: the surface the cut creates. Coating the groove wall with the same selective-contact stack the cell uses elsewhere is a coherent answer, and the fact that it can be done with existing LPCVD capacity and two low-temperature steps is why it is worth watching.

The usual caution applies. The mechanism is sound and follows from established physics; the reported half-point efficiency gain comes from one source and has not been independently confirmed, and the bifaciality figure in particular is weaker than the rest of the table. For a line, the reasonable position is to track it as a process insertion with a real but unverified gain, and to test it on the measurement that the mechanism predicts, which is voltage.

**Related reading:** [TOPCon four-cut cells: what the cut changes](https://www.ooitech.com/topcon-four-cut-cells-how-cutting-a-cell-into-four-increases-power-output.html) · [Four-cut cell technology: the efficiency argument](https://www.ooitech.com/four-cut-cell-technology-the-next-efficiency-code-in-the-pv-industry.html) · [Multi-cut modules and shade resistance](https://www.ooitech.com/multi-cut-solar-modules-a-practical-analysis-of-shade-resistance.html) · [Why four-cut modules need two-part junction boxes](https://www.ooitech.com/why-topcon-four-cut-modules-need-two-part-junction-boxes-a-look-at-pv-junction-box-evolution.html) · [THBC cells and passivating contacts](https://www.ooitech.com/thbc-solar-cell-technology-how-hybrid-passivated-back-contact-breaks-the-28-efficiency-barrier.html) · [PV cell metallisation and the copper question](https://www.ooitech.com/pv-cell-metallization-can-the-silver-blocking-playbook-be-used-to-stop-copper.html) · [Tabber and stringer machines: how they work](https://www.ooitech.com/tabber-and-stringer-machine-how-it-works-how-to-choose.html) · [Laser cell cutting equipment](https://www.ooitech.com/SC-20P-Automatic-Solar-Cell-Laser-Cutting-Machine-High-Precision-BC-Cell-Processing-Equipment.html) · [BC cell roadmap: structure to process](https://www.ooitech.com/bc-cell-technology-roadmap-structure-to-process.html) · [Solar panel line stations and layout](https://www.ooitech.com/solar-panel-manufacturing-machine-stations-and-line-layout.html)

Data note: layer thicknesses, process conditions and the before-and-after comparison are the values published with this route and are reproduced as reported; they have not been independently verified. The wall area figure of about 1 mm2 is our own estimate from a 30 µm groove, a 1.5 µm depth and two full-length cuts on an 182 mm cell, against a wafer face of 33,124 mm2. The ranking of the losses, voltage before current, follows from the mechanism rather than from a printed figure.

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Request A Quote

All uploads are secure and confidential.

## We deliver expertise you can trust our service

Direct-from-Factory Equipment.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Cost-Effective Advantages

We deliver exceptional value, maximizing results while optimizing budgets for clients.

![](/template/ooitech/assets/img/icon/staff.svg)

### Our Experience Team

Our skilled professionals specialize in innovative solutions and tailored strategies.

![](/template/ooitech/assets/img/icon/certified.svg)

### 15+ Years Industry Experience

Deep expertise ensures reliable, trend-aware, and proven outcomes for success.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## What Our Client Say's about us

Client testimonials praise our deep understanding of their challenges, which leads to innovative solutions and strong ROI. Long-term collaborations—some over a decade—demonstrate their trust and satisfaction. Their success stories drive us to continually exceed expectations. [Know More **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

Thanks to Ooitech for providing the fully automated production equipment—your installation and after-sales service have been excellent.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

![](/template/ooitech/assets/img/icon/quote.svg)

A man with a big soul. Thank you very much for your visit Mr Wu. Thank you very much for the services provided in installing equipment and training my students. The kindest person and professional in his field

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

![](/template/ooitech/assets/img/icon/quote.svg)

Thanks to Ooitech for providing highly suitable BC solar cell experimental equipment.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

![](/template/ooitech/assets/img/icon/quote.svg)

thank you for ooitech's professional support and on time after service.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra From Africa

![](/template/ooitech/assets/img/icon/quote.svg)

Thank you again so much again for the very big big help for improving and fixing the factory and also teaching the workers how to use the machines

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

## Our Latest Products

![OTCY-2754DD BIPV Laminator: Double-Chamber, Single-Layer](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774438298752758.webp)

- [** Rachael](./OTCY-2754DD-Single-Layer-Double-Chamber-Automatic-BIPV-Laminator-High-Performance-Solar-Module-Produ.html)
- [** 63609](./OTCY-2754DD-Single-Layer-Double-Chamber-Automatic-BIPV-Laminator-High-Performance-Solar-Module-Produ.html)

### OTCY-2754DD BIPV Laminator: Double-Chamber, Single-Layer

Ooitech solar panel laminator full catalogue: 10 models, technical specs comparison, system descriptions, safety controls

![Solar Cells for PV Modules](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774581692247238.webp)

- [** Rachael](./Professional-Solar-Cell-Solutions-for-Modern-PV-Panel-Manufacturing-Ooitech.html)
- [** 71677](./Professional-Solar-Cell-Solutions-for-Modern-PV-Panel-Manufacturing-Ooitech.html)

### Solar Cells for PV Modules

Solar cell processing equipment for PERC, TOPCon, HJT & BC cells – cutting, stringing, testing. Supports G1/M6/M10/M12 sizes.

![CHT9980A PV Safety Tester: 8kV, 0.001kV Resolution](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032763823477.jpg)

- [** Rachael](./cht9980a-cht9981a-pv-safety-comprehensive-tester-solar-panel-hipot-insulation-ground-continuity-tester.html)
- [** 84115](./cht9980a-cht9981a-pv-safety-comprehensive-tester-solar-panel-hipot-insulation-ground-continuity-tester.html)

### CHT9980A PV Safety Tester: 8kV, 0.001kV Resolution

CHT9980A/CHT9981A PV Safety Comprehensive Tester is a high-performance 3-in-1 instrument integrating DC withstand voltage, insulation resistance

![Low-Temperature PV Ribbon and Flux for Solar Strings](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032717287347.webp)

- [** Rachael](./Solar-Panel-Soldering-Ribbon-and-Flux-Essential-Components-for-PV-Module-Manufacturing.html)
- [** 21332](./Solar-Panel-Soldering-Ribbon-and-Flux-Essential-Components-for-PV-Module-Manufacturing.html)

### Low-Temperature PV Ribbon and Flux for Solar Strings

PV ribbon and flux for solar cell interconnection: low-temperature soldering ribbon in high-purity tin-coated copper, supporting MBB and half-cut lines.

![C350-CQC EVA & TPT Strip Cutting Machine: 30-80mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032714363679.webp)

- [** Rachael](./ECPC-C350-CQC-Punching-and-Cutting-Machine-High-Precision-Solar-Panel-Material-Processing-Equipment.html)
- [** 34867](./ECPC-C350-CQC-Punching-and-Cutting-Machine-High-Precision-Solar-Panel-Material-Processing-Equipment.html)

### C350-CQC EVA & TPT Strip Cutting Machine: 30-80mm

C350-CQC punching & cutting machine – 30 pcs/min, ±0.2mm accuracy for EVA, TPT & PPE solar materials. Precision processing for busbar and

![Solar Tempered Glass: 93.5% Transmittance, Low-Iron](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774514074283403.webp)

- [** ooitech](./Solar-Glass-Ultra-Clear-Low-Iron-Tempered-Glass-for-Photovoltaic-Modules.html)
- [** 47909](./Solar-Glass-Ultra-Clear-Low-Iron-Tempered-Glass-for-Photovoltaic-Modules.html)

### Solar Tempered Glass: 93.5% Transmittance, Low-Iron

Solar tempered glass for PV modules: ultra-clear low-iron glass with anti-reflective coating, reaching 91.5%+ light transmittance in G1/M6/M10/M12 sizes.